Safety information search results
Filter your results
Building or structure type
Building height
Project or lifecycle stage
Operation or occupation
Codes, standards & regulations
Fire incident response
Method of construction
Structural form
Temporary works
Plant & equipment
Weather & natural hazards
Utilities
Safety reporting
Project delivery methods
Business practice
Risk management
Public incidents
Theme pages
Locations
Content type
- CROSS-AUS Newsletter 3 (1)
- CROSS-AUS Newsletter 5 (1)
- CROSS-AUS [sub-heading only] (1)
- CROSS-UK Newsletter 4 (2)
- CROSS-UK Newsletter 11 (1)
- CROSS-UK Newsletter 29 (1)
- CROSS-UK Newsletter 33 (1)
- CROSS-UK Newsletter 34 (1)
- CROSS-UK Newsletter 65 (1)
- CROSS-UK [sub-heading only] (6)
- CROSS Newsletter (4)
- CROSS Safety Report (11)
- News [sub-heading only] (1)
CROSS regions
Poor quality design leads to failure for a small design and build contract
An example of a small design and build contract where poor design and management led to an inadequate structure being built.
6 June 2022
CROSS Safety Report
Report ID: 1088
Region: CROSS-UK
Failure of large aluminium composite panel
This report highlights the importance of correctly designed fixings and anchoring systems for cladding panels to buildings to minimize the risk of failure.
30 April 2021
CROSS Safety Report
Report ID: 962
Region: CROSS-AUS
Possible galvanising concern
A reporter has a question about using galvanised steel poles for the members of dome structures.
1 November 2006
CROSS Safety Report
Report ID: 48
Region: CROSS-UK
Liquid metal assisted cracking (LMAC)
A reporter raises concerns about the risk of liquid metal assisted cracking during the hot dip galvanising process.
1 November 2006
CROSS Safety Report
Report ID: 45
Region: CROSS-UK
Follow up to Liquid Metal Assisted Cracking (LMAC)
A recent case involving cracking around holes in large structural components was detected immediately after galvanising as a result of the team being aware of the need for post galvanising inspection.
1 July 2008
CROSS Safety Report
Report ID: 105
Region: CROSS-UK
Freezing splits galvanised SHS columns
Concerns were raised after several square hollow section members split vertically on a partially complete construction site.
1 April 2012
CROSS Safety Report
Report ID: 253
Region: CROSS-UK
Documentation for imported large diameter steel pins
A reporter raises concerns over the possibility that foreign steel with poor, confusing or misleading documentation, is being used on safety critical structures in the UK.
1 January 2013
CROSS Safety Report
Report ID: 299
Region: CROSS-UK
Further issues with freezing and galvanised hollow sections
A reporter was involved in correcting a cold formed galvanised square hollow section (SHS) four storey balcony structure where longitudinal splits formed in at least two of the four columns.
1 January 2014
CROSS Safety Report
Report ID: 314
Region: CROSS-UK
Grades of weldable quality bolts
A reporter says grade 8.8 bolts are not required to be manufactured as being weldable according to the relevant product standards e.g. ISO 898-1 and -2.
1 April 2014
CROSS Safety Report
Report ID: 392
Region: CROSS-UK
Dislodged finger plate on highway bridge
A correspondent received a report about a 1.5m long section of a steel finger plate expansion joint on a highway bridge that had been inadequately fixed and became dislodged.
1 February 2020
CROSS Safety Report
Report ID: 879
Region: CROSS-AUS
Submit a report
Your report will make a difference. It will help to create positive change and improve safety.
Our secure and confidential safety reporting system gives professionals the opportunity to share their experiences to help others.